Hostname: page-component-cb9f654ff-c75p9 Total loading time: 0 Render date: 2025-08-28T00:56:09.350Z Has data issue: false hasContentIssue false

Quasi-static and Dynamic Nanoindentation Testing of Lamellar and Inter-lamellar Trabecular Bone

Published online by Cambridge University Press:  10 February 2011

Thorsten Staedler
Affiliation:
Department of Materials Science and Engineering, Cornell University, Ithaca, NY
Eve Donnelly
Affiliation:
Sibley School of Mechanical and Aerospace Engineering, Cornell University, Ithaca, NY
Marjolein C. H. van der Meulen
Affiliation:
Sibley School of Mechanical and Aerospace Engineering, Cornell University, Ithaca, NY
Shefford P. Baker
Affiliation:
Department of Materials Science and Engineering, Cornell University, Ithaca, NY
Get access

Abstract

Bone is a complex natural composite with a lamellar structure on the micro scale. In this study, scanning nanoindentation was used to assess the mechanical properties of individual lamellar and inter-lamellar components of trabecular bone under static and dynamic loading conditions. The combination of careful sample preparation, good topographical characterization of the sample surface, and a scanning nanoindenter provided insight into the mechanical properties of the individual lamellar structures. The results of quasi-static, as well as dynamic nanoindentation tests of bone are reported and discussed.

A surface roughness of only 18-20 nm RMS was achieved. Nonetheless, indentation depths in the range of 100 nm and above were required in order to minimize the effect of topography on the measurement. This requirement conflicts with the need to keep the probed volume small enough to sample only one component at a time. A simple volume-averaging model was developed and used as a tool to determine when individual lamellar bone structures were being probed and to help determine the properties of the lamellar and inter-lamellar materials.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1 Dickson, I.R., in Connective Tissue and its Heritable Disorders (Royce, P.M. and Steinmann, B., eds.), 249285 (1993)Google Scholar
2 Howell, P.G.T. and Boyde, A., Scanning 21, 361 (1999)Google Scholar
3 Hengsberger, S., Kulik, A., and Zysset, P.K., European Cells and Materials 1, 12 (2001)Google Scholar
4 Kinney, J.H., Haupt, D.L., Balooch, M., Ladd, A.J., Ryaby, J.T., and Lane, N.E., Journal of Bone and Mineral Research 15, 1981 (2000)Google Scholar
5 Hengsberger, S., Kulik, A., and Zysset, P.K., Bone 30, 178 (2002)Google Scholar
6 Boyde, A and Hobdell, M.H., Zeitschrift für Zellforschung und mikroskopische Anatomie 93, 213 (1969)Google Scholar
7 Marotti, G., Calcified Tissue International 53, S47 (1993)Google Scholar
8 Weiner, S., Arad, T., Sabanay, I., and Traub, W., Bone 20, 509 (1997)Google Scholar
9 Giraud-Guille, M.M., Calcified Tissue International 42, 167 (1988)Google Scholar
10 Rho, J.-Y., Tsui, T.Y., and Pharr, G.M., Biomaterials 18, 1325 (1997)Google Scholar
11 Rho, J.-Y. and Pharr, G.M., Journal of Materials Science: Materials in Medicine 10, 485 (1999)Google Scholar
12 Zysset, P.K., Guo, X.E., Hoffler, C.E., Moore, K.E., and Goldstein, S.A., Journal of Biomechanics 32, 1005 (1999)Google Scholar
13 Hoffler, C.E., Moore, K.E., Kozloff, K., Zysset, P.K., Brown, M.B., and Goldstein, S.A., Bone 26, 603 (2000)Google Scholar
14 Donnelly, E., Staedler, T., Baker, S.P, and van der Meulen, M.C.H., Proceedings of the 49th Annual Meeting of the Orthopedic Research Society, NewOrleans, LA, 2003 Google Scholar
15 Baker, S.P., Thin Solid Films 308-309, 289 (1997)Google Scholar
16 Oliver, W.C. and Pharr, G.M., Journal of Materials Research 7, 1564 (1992)Google Scholar
17 Loubet, J.-L., Lucas, B.N., and Oliver, W.C., NIST Special Publications 896, (1996)Google Scholar
18 Staedler, T., Donnelly, E., van der Meulen, M.C.H., and Baker, S.P, submitted to Journal of Materials ResearchGoogle Scholar