Hostname: page-component-7c8c6479df-ph5wq Total loading time: 0 Render date: 2024-03-28T20:18:21.562Z Has data issue: false hasContentIssue false

Self-Assembling Peptide Monolayers: Endothelial Cell Behavior on Functionalized Metal Substrates

Published online by Cambridge University Press:  15 February 2011

E.L. Chaikof
Affiliation:
Department of Surgery, Emory University, Atlanta, GA 30322, echaikof@surgery.eushc.org School of Chemical Engineering, Georgia Institute of Technology, Atlanta, GA 30322
H. S. Wang
Affiliation:
Department of Surgery, Emory University, Atlanta, GA 30322, echaikof@surgery.eushc.org
T. M. Wingert
Affiliation:
School of Chemical Engineering, Georgia Institute of Technology, Atlanta, GA 30322
S. Stephens
Affiliation:
Department of Chemistry, University of Georgia, Athens, GA 30602
R. A. Dluhy
Affiliation:
Department of Chemistry, University of Georgia, Athens, GA 30602
Get access

Abstract

Despite the high initial success rate with metallic stents for the treatment of a variety of vascular lesions, problems have included occlusion due to thrombus formation or intimal proliferation. Improving the biological behavior of these and other other implantable metallic devices may require the use of biomimetic peptide coatings which promote specific cellular responses at the biological-materials interface.

Thiol-terminated peptides, without the addition of a cysteine residue, were synthesized by a modification of standard solid phase methodology. Gold/mica or gold/glass surfaces were exposed for 6 hours at 23 °C to one of three peptide solutions: GRGD(βA)3YNH(CH2)2SH (RGD); (βA)6NH (CH2)2SH (bAla); or a 1:1 mix of both peptides. Peptide films were examined by external reflectance infrared (IR) spectroscopy and atomic force microscopy (AFM) which confirmed the presence of unique close-packed structures for bAla and the 1:1 mix. Endothelial cell proliferative, migratory, and adhesive behavior were evaluated using 3H-thymidine and 51Cr labeling techniques, respectively. Cell proliferation, migration, and adhesion were significantly higher on RGD containing peptide films.

Well-ordered protein assemblies on metallic substrates can be produced with the proper choice of peptide chain structure and terminal residues. Biological activity is a function of film composition and oligopeptide pendant structure.

Type
Research Article
Copyright
Copyright © Materials Research Society 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Ulman, A., An Introduction to Ultrathin Organic Films. From Langmuir-Blodgett to Self-Assembly. (Academic Press, New York, 1991), pp. 237301.Google Scholar
2. Fraser, R. D. B., MacRae, T. P., Rogers, G. E., Keratins: Their Composition. Structure and Biosynthesis. (C. C. Thomas, Springfield, IL, 1972), pp. 83120.Google Scholar
3. Winger, T. M., Ludovice, P. J., Chaikof, E. L., Bioconj. Chem. 6, p. 323 (1995).Google Scholar
4. Whitesell, J. K., Chang, H. K.. Science 261, p. 7376 (1993).Google Scholar
5. Enriquez, E. P., Samulski, E. T. in Hierarchically Structured Materials, edited by Aksay, I. A., Baer, E., Sarikaya, M., Tirrell, D. A. (Mater. Res. Soc. Proc. 255, Pittsburgh, PA, 1992) p. 423434.Google Scholar