Hostname: page-component-76fb5796d-9pm4c Total loading time: 0 Render date: 2024-04-25T23:27:08.774Z Has data issue: false hasContentIssue false

Structural and Hydriding/Dehydriding Properties of HoMn2Hx with Cubic and Hexagonal Laves Phase Structure

Published online by Cambridge University Press:  01 February 2011

Yoshikazu Makihara
Affiliation:
makihara@kyukyo-u.ac.jp, Kyushu Kyoritsu University, Mechanical and Electronic System Engineering, 1-8 Jiyugaoka, yahatanishi-ku, Kitakyushu, N/A, 807-8585, Japan
Youichi Iwata
Affiliation:
04a7102@edu.cc.kyukyo-u.ac.jp, Kyushu Kyoritsu University, Department of Mechanical and Electronic System Engineering, 1-8 Jiyugaoka, Yahatanishi-ku, Kitakyushu, N/A, 807-8585, Japan
Kazumi Umeda
Affiliation:
04a7701@edu.cc.kyukyo-u.ac.jp, Kyushu Kyoritsu University, Department of Mechanical and Electronic System Engineering, 1-8 Jiyugaoka, Yahatanishi-ku, Kitakyushu, N/A, 807-8585, Japan
Yoshio Miyairi
Affiliation:
miyairi@kyukyo-u.ac.jp, Kyushu Kyoritsu University, Department of Mechanical and Electronic System Engineering, 1-8 Jiyugaoka, Yahatanishi-ku, Kitakyushu, N/A, 807-8585, Japan
Hironobu Fujii
Affiliation:
hfujii@hiroshima-u.ac.jp, Hiroshima University, Natural Science Center for Basic Research and Development, 1-3-1 Kagamiyama, Higashi-Hiroshima, N/A, 739-8526, Japan
Get access

Abstract

Both the cubic C15-type and the hexagonal C14-type Laves phase compounds HoMn2 were successfully prepared. We found that they absorbed hydrogen up to 3.4 atoms per formula unit at room temperature and discharged it at around 490 K, reversibly. Structural and hydriding/dehydriding properties of the host HoMn2 and their hydrides HoMn2Hx have been investigated by powder X-ray diffraction (XRD) and thermogravimetry/differential thermal analysis (TG/DTA). With increasing the hydrogen content, the host C15-type HoMn2 is distorted into a rhombohedral phase at above x = 2.9, while the host C14-type one keeps the hexagonal structure up to x = 3.4. The experimental results obtained from TG/DTA measurement suggest that two possible interstitial sites with different activation energies for hydrogen desorption exist in the C14 HoMn2, while one site in the C15 HoMn2.

Type
Research Article
Copyright
Copyright © Materials Research Society 2006

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Shaltiel, D., Jacob, I. and Davidov, D., J. Less-Common Met. 53, 117 (1977).Google Scholar
2. Pebler, A. and Gulbransen, E.A., Electrochem. Technol. 4(5-6), 211 (1966).Google Scholar
3. Fruchart, D., Roualt, A., Shoemaker, C.B. and Shoemaker, D.P., J. Less-Common Met. 73, 363 (1980).Google Scholar
4. Soubeyroux, J.L., Bououdina, M., Fruchart, D. and Pontonnier, L., J. Alloys Comp. 219, 48 (1995).Google Scholar
5. Przewoznik, J., Zukrowski, J., and Krop, K., J. Magn. Magn. Mater. 140–144, 807 (1995).Google Scholar
6. Zukrowski, J., Figiel, H., Budziak, A., Zachariasz, P., Fischer, G., and Dormann, E., J. Magn. Magn. Mater. 238, 129 (2002).Google Scholar
7. Figiel, H., Budziak, A., Zukrowski, J., Fischer, G., Kelemen, M.T., and Dormann, E., J. Alloys Comp. 335, 48 (2002).Google Scholar
8. Przewoznik, J., Zukrowski, J., Freindl, K., Japa, E., and Krop, K., J. Alloys Comp. 284, 31 (1999).Google Scholar
9. Goncharenko, I.N., Mirebeau, I., Irodova, A.V. and Suard, E., Phys. Rev. B 59, 9324 (1999)Google Scholar
10. Makihara, Y., Andoh, Y., Hashimoto, Y., Fujii, H., Hasuo, M. and Okamoto, T., J. Phys. Soc. Jpn. 52, 629 (1983)Google Scholar