Hostname: page-component-848d4c4894-2pzkn Total loading time: 0 Render date: 2024-05-06T02:13:33.670Z Has data issue: false hasContentIssue false

Synthesis of La4Ni3O10 Cathode Material (SOFC) by SOL-GEL Process

Published online by Cambridge University Press:  01 February 2011

Rene Fabian Cienfuegos
Affiliation:
Fac. Ing. Mec. Eléc. (FIME), San Nicolás de los Garza, Nuevo León, 66451, México Cent. Innov., Invest. Desar. Ing. Tec. (CIIDIT), Apodaca, Nuevo León, 66600, México
Sugeheidy Carranza
Affiliation:
Fac. Ing. Mec. Eléc. (FIME), San Nicolás de los Garza, Nuevo León, 66451, México
Leonardo Chávez
Affiliation:
Fac. Ing. Mec. Eléc. (FIME), San Nicolás de los Garza, Nuevo León, 66451, México Cent. Innov., Invest. Desar. Ing. Tec. (CIIDIT), Apodaca, Nuevo León, 66600, México
Laurie Jouanin
Affiliation:
Université Paris-Sud 11,Orsay, 91405, France.
Guillaume Marie
Affiliation:
IUT A de Lille, Boul. Paul LANGEVIN, BP 179, Villeneuve d'Ascq Cedex, 59653, France
Moisés Hinojosa
Affiliation:
Fac. Ing. Mec. Eléc. (FIME), San Nicolás de los Garza, Nuevo León, 66451, México Cent. Innov., Invest. Desar. Ing. Tec. (CIIDIT), Apodaca, Nuevo León, 66600, México
Get access

Abstract

The goal in this study is to synthesize a Ruddleden-Poper La-Ni phase (La4Ni3O10) using a polymeric route. This material exhibits mixed ionic and electronic conduction (MIEC) properties and can be used as cathode material in the manufacture of Solid Oxide Fuel Cells (SOFC). In addition, an easy and inexpensive synthesis method is presented The polymeric precursors are prepared following the Castillo method using optimized the complexation ratios (HMTA/metallic salts) from 1 to 6. The obtained powders are characterized by differential scanning calorimetry (DSC), thermogravimetric analysis (TGA) and X-ray diffraction (XRD) in order to determine the processing conditions for formation of the crystalline phase. Experiments performed using complexation ratios of 5 and 6 do not show coagulation. However, the solution prepared using a complexation ratio of 5, is transformed into a gel after few days. Gels produced from solutions prepared with complexation ratios from 2 to 5 were heated at 800, 900 and 1000°C to obtain solid materials. These powders are characterized by TGS, DSC and XRD and it is found that the temperature needed to obtain crystalline La4Ni3O10 was 1000°C.

Type
Research Article
Copyright
Copyright © Materials Research Society 2010

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Mauvy, F., Lalanne, C., Bassat, J.M., Grenier, J.C., Zhao, H., Dordor, P. and Stevens, Ph., Journal of the European Ceramic Society 25, 26692672 (2005)Google Scholar
2. Castillo, S., Cienfuegos, R.F., Fontaine, M.L., Lenormand, P., Bacchin, P. and Ansart, F., Materials Research Bulletin 42, 21252131 (2007)Google Scholar
3. Marie-Laure, Fontaine, Christel, Laberty-Robert, Antoine, Barnabé, Florence, Ansart and Philippe, Tailhades, Ceramics International 30, 20872098 (2004)Google Scholar
4. Nesaraj, S., Journal of Scientific & Industrial Research, 69, 169176 (2010)Google Scholar
5. Wincewicz, K.C. and Joyce Cooper, S., Journal of Power Sources, 140, 280296 (2005)Google Scholar
6. Chunwen, Sun, Rob, Hui and Justin, Roller, J Solid State Electrochem, 14, 11251144 (2010)Google Scholar
7. Cienfuegos, R. F., D. Thesis, Université Toulouse III, 2008,Google Scholar