Hostname: page-component-857557d7f7-ktsnh Total loading time: 0 Render date: 2025-11-26T00:11:27.367Z Has data issue: false hasContentIssue false

Epoxy based composite surface analysis. A plasma treatmentfor wettability evolution

Published online by Cambridge University Press:  11 December 2009

J.-F. Coulon*
Affiliation:
École Louis de Broglie, Groupe ECAM, Campus de Ker Lann, 35170 Bruz, France
H. Maillard
Affiliation:
École Louis de Broglie, Groupe ECAM, Campus de Ker Lann, 35170 Bruz, France
Get access

Abstract

Manufactured carbon/epoxy composite surfaces were analysed before and after CF4 plasma treatment in order to study their wettability with the aim to master adhesion properties. Roughness and XPS surface composition on raw and plasma treated surfaces have been correlated to surface free energy measurements. The analytical tools were first validated on a flat epoxy resin before being tested and compared on rough industrial carbon/epoxy composite samples. The results reveal that these analytical techniques can be reproducible and relevant on manufactured composite for new surface treatment studies.

Keywords

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

Amouroux, J., Arefi, F., Polym. Mater. Sci. Eng. 62, 418 (1990)
Poncin-Epaillard, F., Legeay, G., Ann. Chim. Sci. Mat. 28, 55 (2003) CrossRef
Legeay, G., Poncin-Epaillard, F., Arciola, C.R., Int. J. Art. Organs 29, 453 (2006)
Yan, Y.H., Chan-Park, M.B., Hue, C.Y., Langmuir 21, 8905 (2005) CrossRef
Manca, M., Cortese, B., Viola, I., Arico, A., Cingolani, R., Gigli, G., Langmuir 24, 1833 (2008) CrossRef
Coulon, J.F., Turban, G., Rabinzohn, P., Jeannerot, L., J. Vac. Sci. Technol. A 10, 3076 (1992) CrossRef
P.G. de Gennes, F. Brochard-Wyart, D. Quéré, Gouttes, bulles, perles et ondes (Belin, Paris, 2005)
Owens, D.K., Wendt, R.C., J. Appl. Polym. Sci. 13, 1741 (1969) CrossRef
Van Oss, C., Chaudhury, M.K., Good, R.J., Chem. Rev. 88, 927 (1988) CrossRef
Good, R.J., J. Adhesion Sci. Technol. 6, 1269 (1992) CrossRef
Della Volpe, C., Siboni, S., J. Adhesion Sci. Technol. 14, 235 (2000) CrossRef
Brostow, W. et al., Polym. Int. 52, 1498 (2003) CrossRef
J.F. Coulon, Ph.D. thesis, University of Nantes, 1992
Bénard, Q., Fois, M., Grisel, M., Appl. Surf. Sci. 253, 4753 (2007) CrossRef
Bhowmik, S., Bonin, H.W., Bui, V.T., Weir, R.D., J. Appl. Polym. Sci. 102, 1959 (2006) CrossRef
Bico, J., Tordeux, C., Quéré, D., Europhys. Lett. 55, 214 (2001) CrossRef
Lafuma, A., Quéré, D., Nat. Mater. 2, 457 (2003) CrossRef