Summary

Electrons reflected from a crystal surface are generated by two scattering mechanisms. Bragg reflection, which is purely an elastic scattering process, is responsible for producing sharp peaks governed by Bragg's law. Inelastic scattering, which is dominated by valence-loss and thermal diffuse scattering (TDS), contributes a Kikuchi pattern background in the electron angular distribution and results in electron energy losses and momentum transfers. The excitation of Bragg reflections critically depends on the diffracting conditions, and the intensity distribution in a RHEED pattern is the result of dynamical scattering of electrons by the crystal surface. It is thus important to understand how electrons are reflected from the surface in order to illustrate the surface sensitivity of REM.

In this chapter, the physics of surface resonance in RHEED are systematically illustrated. Experimental results will be shown to exhibit the nature of surface resonance. It will be demonstrated that the surface sensitivity of RHEED will be dramatically enhanced by resonance. Finally, the effect of inelastic scattering on resonance reflection will be discussed.

The phenomenon

Surface resonance is one of the most important scattering processes in RHEED and REM. The surface resonance effect was first observed by Kikuchi and Nakagawa (1933); the reflected-electron intensity suddenly increases when the diffraction spot crosses an oblique Kikuchi line. This is illustrated by the RHEED pattern shown in Figure 4.1. When the resonance condition is not satisfied, there is no strongly reflected beam (Figure 4.1 (a)). The intensity is increased by almost an order of magnitude if the surface resonance is excited (Figure 4.1(b)).

Information

Type
Chapter
Information
Publisher: Cambridge University Press
Print publication year: 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Accessibility standard: Unknown

Why this information is here

This section outlines the accessibility features of this content - including support for screen readers, full keyboard navigation and high-contrast display options. This may not be relevant for you.

Accessibility Information

Accessibility compliance for the PDF of this book is currently unknown and may be updated in the future.

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Resonance reflections in RHEED
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.006
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Resonance reflections in RHEED
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.006
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Resonance reflections in RHEED
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.006
Available formats
×