Grain refinement effect of a pulsed magnetic field on as-cast superalloy K417

Published online by Cambridge University Press:  31 January 2011

Yuansheng Yang*
Affiliation:
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, People's Republic of China
*
a) Address all correspondence to this author. e-mail: ysyang@imr.ac.cn
Get access

Abstract

The grain refinement effect of a pulsed magnetic field on superalloy K417 was studied. The experimental results show that fine equiaxed grains are acquired with proper thermal control under the pulsed magnetic field. The refinement effect of the pulsed magnetic field is affected by the melt cooling rate and the melt superheating. The refinement effect of the pulsed magnetic field is attributed to the dissociation of nuclei from the mold wall by melt vibration and the subsequent dispersion of nuclei by melt convection. The Joule heat and the melt convection caused by the pulsed magnetic field may defer the formation of solidified shell, which prolongs the continuous refinement process. The decrease of melt cooling rate reduces the number of nuclei produced on the mold wall but prolongs the duration for the nuclei to depart from the mold wall and disperse in the melt, which enhances the refinement effect of the pulsed magnetic field. The increase of melt superheating lessens the survival probability of the nuclei in the melt, which weakens the refinement effect of the pulsed magnetic field.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1Woulds, M. and Benson, H.: Development of a conventional fine grain casting process, in Proceedings of the Superalloy 1984, edited by Gellm, M. (Met. Soc. TMS-AIME, New York, 1984), p. 3.Google Scholar
2Chang, E., Tseng, B., Chou, J.C., and Yin, V.: Processing structure and mechanical property of investment cast IN713LC superalloy. AFS Trans. 96, 47 (1988).Google Scholar
3Mondolfo, L.F.: Grain refinement in the casting of non-ferrous alloys, in Grain Refinement in Casting and Welds, edited by Addaeshian, G.J. (TMS-AIME, Warrendale, PA, 1983), p. 3.Google Scholar
4Ewing, B.A. and Green, K.A.: Polycrystalline grain controlled castings for rotating compressor and turbine components, in Superalloys 1984, edited by Gell, M. (TMS-AIME, Warrendale, PA, 1984), p. 33.Google Scholar
5Bouse, G.K. and Behrendt, M.R.: Mechanical properties of microcast-X alloy 718 fine grain investment castings, in Superalloy 718–Metallurgy and Applications, edited by Loria, E. (Met. Soc., Warrendale, PA, 1989), p. 319.Google Scholar
6Vives, C.: Effects of electromagnetic vibrations on the microstructure of continuously cast aluminum alloys. Mater. Sci. Eng., A 173, l69 (1993).Google Scholar
7Radjai, A. and Miwa, K.: Effects of the intensity and frequency of electromanetic vibrations on the microstructural refinement of hypereutectic Al-Si alloys. Metall. Mater. Trans. A 31, 755 (2000).CrossRefGoogle Scholar
8Mizutani, Y., Tamura, T., and Miwa, K.: Microstructural refinement process of pure magnesium by electromagnetic vibrations. Mater. Sci. Eng., A 413–414, 205 (2005).CrossRefGoogle Scholar
9Zi, B.T., Ba, Q.X., Cui, J.Z., Bai, Y.G., and Yan, X.J.: Effect of strong pulsed electromagnetic field on metal's solidified structure. Acta Phys. Sin. 49, 1010 (2000).Google Scholar
10Gao, Y.L., Li, Q.S., Gong, Y.Y., and Zhai, Q.J.: Comparative study on structural transformation of low-melting pure Al and highmelting stainless steel under external pulsed magnetic field. Mater. Lett. 61, 4011 (2007).CrossRefGoogle Scholar
11Li, Q.S., Song, C.J., Li, H.B., and Zhai, Q.J.: Effect of pulsed magnetic field on microstructure of 1Cr18Ni9Ti austenitic stainless steel. Mater. Sci. Eng., A 466, 101 (2007).CrossRefGoogle Scholar
12Zhou, Q., Yang, Y.S., and Ma, J.C.: Effect of pulsed magnetic field on solidified structure of AZ91D magnesium alloy. Foundry 56, 148 (2007).Google Scholar
13Wang, B., Yang, Y.S., Zhou, J.X., and Tong, W.H.: Microstructure refinement of AZ91D alloy solidified with pulsed magnetic field. Trans. Nonferrous Met. Soc. China 18, 536 (2008).CrossRefGoogle Scholar
14Southin, R.T.: Nucleation of the equiaxed zone in cast metals. Trans. TMS. 239, 220 (1976).Google Scholar
15Chalmers, B.: Principle of Solidification (John Wiley, New York, 1964), p. 259.Google Scholar
16El-Bassyouni, T.A., Badr, A.A., Abdelm-Azim, A.N., Lakner, J., and Olah, Z.: Effect of electromagnetic forces on aluminum cast structure. Light Metals 33, 733 (1983).CrossRefGoogle Scholar
17Zi, B.T., Yao, K.F., Xu, G.M., and Cui, J.Z.: Numerical simulation of liquid alloy flow field during solidification under applied pulsed magnetic fields. Acta Phys. Sin. 52, 115 (2003).Google Scholar
18Ohno, A.: Solidification—The Separation Theory and Its Practical Applications (Springer-Verlag, Berlin, 1987), p. 15.Google Scholar
19Ohno, A., Motegi, T., and Soda, H.: Origin of the equiaxed crystals in castings. Trans. ISIJ 11, 18 (1971).CrossRefGoogle Scholar
20Herlach, D.M., Eckler, K., Karma, A., and Schwarz, M.: Grain refinement through fragmentation of dendrites in undercooled melts. Mater. Sci. Eng., A 304–306, 20 (2001).CrossRefGoogle Scholar