Novel ultra nanoindentation method with extremely low thermal drift: Principle and experimental results

Published online by Cambridge University Press:  31 January 2011

J. Nohava
Affiliation:
CSM Instruments SA, Rue de la Gare 4, Peseux CH-2034, Switzerland
N.X. Randall*
Affiliation:
CSM Instruments Inc., Needham, Massachusetts 02494
N. Conté
Affiliation:
CSM Instruments SA, Rue de la Gare 4, Peseux CH-2034, Switzerland
*
a) Address all correspondence to this author. e-mail: ra@csm-instruments.com
Get access

Abstract

Despite active development over the past 15 years, contemporary nanoindentation methods still suffer serious drawbacks, particularly long thermal stabilization and thermal drift, which limit the duration of the measurements to only a short period of time. The presented work introduces a novel ultra nanoindentation method that uses loads from the μN range up to 50 mN, is capable of performing long-term stable measurements, and has negligible frame compliance. The method is based on a novel patented design, which uses an active top referencing system. Several materials were used to demonstrate the performance of the method. The measurements with hold at maximum load confirm extremely low levels of instrument thermal drift. The presented Ultra Nanoindentation Tester opens new possibilities for testing thin films and long-term testing, including creep of polymers at high resolution without the need of long thermal stabilization.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Schwarzer, N., Chudoba, T., and Richter, F.: Investigation of ultra thin coatings using nanoindentation. Surf. Coat. Technol. 200, 5566 (2006).CrossRefGoogle Scholar
2.Fischer-Cripps, A.C.: The IBIS Handbook of Nanoindentation (Fischer-Cripps Laboratories Pty Ltd., Australia, 2005), p. 60.Google Scholar
3.Zhang, R. and Ma, H.: Nano-mechanical properties and nanotribological behaviors of nitrogen-doped diamond-lie carbon (DLC) coatings. J. Mater. Sci. 41, 1705 (2006).Google Scholar
4.Chudoba, T. and Richter, F.: Investigation of creep behaviour under load during indentation experiments and its influence on hardness and modulus results. Surf. Coat. Technol. 148, 191 (2001).CrossRefGoogle Scholar
5.ASTM E 2546–07: Standard practice for instrumented indentation testing.Google Scholar
6.ISO 14577: Metallic materials—Instrumented indentation test for hardness and material parameters.Google Scholar
7.Randall, N.X., Christoph, R., Droz, S., and Julia-Schmutz, C.: Localized micro-hardness measurements with a combined scanning force microscope/nanoindentation system. Thin Solid Films 290–291, 348 (1996).CrossRefGoogle Scholar
8.Randall, N.X., Julia-Schmutz, C., Soro, J.M., von Stebut, J., and Zacharie, G.: Novel nanoindentation method for characterizing multiphase materials. Thin Solid Films 308–309, 297 (1997).CrossRefGoogle Scholar
9.Wang, F. and Kewei, X.: An investigation of nanoindentation creep in polycrystalline Cu thin film. Mater. Lett. 58, 2345 (2004).Google Scholar
10.Woirgard, J., Bellaton, B., and Consiglio, R.: U.S. Patent No. WO 2006/069847 A1, July 6, 2006.Google Scholar
11.Fischer-Cripps, A. C.: Nanoindentation (Springer-Verlag), p. 198.Google Scholar
12.Fischer-Cripps, A.C., Karvankova, P., and Veprek, S.: On the measurement of hardness of super-hard coatings. Surf. Coat. Technol. 200, 5645 (2006).CrossRefGoogle Scholar
13.Oliver, W.C. and Pharr, G.M.: Measurement of hardness and elastic modulus by instrumented indentation: Advances in understanding and refinements to methodology. J. Mater. Res. 19(1), 3 (2004).CrossRefGoogle Scholar
14.Lucas, B.N., Oliver, W.C., Pharr, G.M., and Loubet, J-L.: Time dependent deformation during indentation testing, in Thin Films: Stresses and Mechanical Properties VI, edited by Gerberich, W.W., Gao, H., Sundgren, J-E., and Baker, S.P. (Mater. Res. Soc. Symp. Proc. 436, Pittsburgh, PA, 1997), p. 233.Google Scholar
15.Chen, J. and Bull, S.J.: Assessment of the toughness of thin coatings using nanoindentation under displacement control. Thin Solid Films 494, 1 (2006).CrossRefGoogle Scholar
16.Page, T.F., Oliver, W.C., and McHargue, C.J.: The deformation behavior of ceramic crystals subjected to very low load (nano) indentations. J. Mater. Res. 7(2), 450 (1992).CrossRefGoogle Scholar
17.Oliver, W.C. and Pharr, G.M.: An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7(6), 1564 (1992).CrossRefGoogle Scholar
18.Van Vliet, K., Prchlik, L., and Smith, J.F.: Direct measurement of indentation frame compliance. J. Mater. Res. 19(1), 325 (2004).CrossRefGoogle Scholar
19.Tweedie, C.A. and Van Vliet, K.: Contact creep compliance of viscoelastic materials via nanoindentation. J. Mater. Res. 21(6), 1576 (2006).CrossRefGoogle Scholar
20.Feng, G. and Ngan, A.H.W.: Effects of creep and thermal drift on modulus measurement using depth-sensing indentation. J. Mater. Res. 17(3), 660 (2002).CrossRefGoogle Scholar
21.Beegan, D., Chowdhury, S., and Laugier, M.T.: The nanoindentation behaviour of hard and soft films on silicon substrates. Thin Solid Films 466, 167 (2004).CrossRefGoogle Scholar