Characterization of mechanical properties of tungsten carbide/carbon multilayers: Cross-sectional electron microscopy and nanoindentation observations

Published online by Cambridge University Press:  31 January 2011

N. J. M. Carvalho
Affiliation:
Department of Applied Physics, Materials Science Center and Netherlands Institute of Metals Research, University of Groningen, Nijenborgh 4, 9747 AG Groningen, The Netherlands
J. Th. M. De Hosson*
Affiliation:
Department of Applied Physics, Materials Science Center and Netherlands Institute of Metals Research, University of Groningen, Nijenborgh 4, 9747 AG Groningen, The Netherlands
*
a)Address all correspondence to this author.hossonj@phys.rug.nl
Get access

Abstract

Multilayers of tungsten carbide/carbon (WC/C) deposited by physical vapor deposition onto steel substrates were subjected to depth-sensing indentation testing. The investigation aimed at probing the influence of dissimilarities between the microstructure of the multilayers and substrate on the system mechanical properties. The resultant load-displacement data were analyzed both by conventional load-displacement (P-δ) and load-displacement squared (P2) plots. Furthermore, it was demonstrated that the occurrence of annular through-thickness cracks around the indentation sites can be identified from the load-displacement curve. Also, analysis of the lower part of the unloading curve permitted us to identify whether the coating had popped up by localized fracture. The cracking mechanism was characterized using a new technique for cross-sectional electron microscopy of the nanoindentations. The information retrieved with this technique eliminates the problems, inherent in assessing at this small contact scales, whether the fracture is by coating decohesion or by interfacial failure. In our case, it was demonstrated that the failure mechanism was decohesion of the carbon lamellae within the multilayers. The mechanical properties (hardness and effective Young's modulus) were also assessed by nanoindentation. The hysteresis loops were analyzed and discussed in terms of the method developed by Oliver and Pharr [J. Mater. Res. 7, 1564 (1992)].

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1Güttler, J. and Reschke, J., Surf. Coat. Technol. 60, 531 (1993).CrossRefGoogle Scholar
2Matthews, A. and Eskildesn, S.S., Diamond Relat. Mater. 3, 902 (1994).CrossRefGoogle Scholar
3Wänstrand, O., Larsson, M., and Hedenqvist, P., Surf. Coat. Technol. 111, 247 (1999).CrossRefGoogle Scholar
4Pharr, G.M., Mater. Sci. Eng. A 253, 151 (1998).CrossRefGoogle Scholar
5Page, T.F. and Hainsworth, S.V., Surf. Coat. Technol. 61, 201 (1993).CrossRefGoogle Scholar
6Wright, T. and Page, T.F., Surf. Coat. Technol. 54–55, 557 (1992).CrossRefGoogle Scholar
7Randall, N.X., Schmutz, C.J., and Soro, J.M., Surf. Coat. Technol. 108–109, 489 (1998).CrossRefGoogle Scholar
8Hainsworth, S.V., McGurk, M.R., and Page, T.F., Surf. Coat. Technol. 102, 97 (1998).CrossRefGoogle Scholar
9McGurk, M.R., Chandler, H.W., Twigg, P.C., and Page, T.F., Surf. Coat. Technol. 68–69, 576 (1994).CrossRefGoogle Scholar
10Carvalho, N.J.M. and De Hosson, J.Th.M., Thin Solid Films 388, 150 (2001).CrossRefGoogle Scholar
11Li, K., Wu, T.W., and Li, J.C.M., in Thin Films: Stresses and Mechanical Properties VI, edited by Gerberich, W.W., Sundgren, J-E., Gao, H., and Baker, S.P. (Mater. Res. Soc. Proc. 436, Pittsburgh, PA, 1997), p. 165.Google Scholar
12Sakai, M., Acta Metal. Mater. 41, 1751 (1993).CrossRefGoogle Scholar
13Pharr, G.M., Oliver, W.C., and Brotzen, F.R., J. Mater. Res. 7, 613 (1992).CrossRefGoogle Scholar
14Oliver, W.C. and Pharr, G.M., J. Mater. Res. 7, 1564 (1992).CrossRefGoogle Scholar
15Carvalho, N.J.M., Huis in‘t Veld, A.J., Vellinga, W.P., and De Hosson, J.Th.M., in Surface and Modification Technologies XII: Micro and Nanoindentation Studies of PVD TiN Coated Tool Steel, edited by Sudarshan, T.S., Khor, K.A., Jeandin, M., and Stiglich, J. (ASM, Materials Park, Ohio, 1998), p. 25.Google Scholar
16Whitehead, A.J. and Page, T.F., Thin Solid Films 220, 277 (1992).CrossRefGoogle Scholar
17Hainsworth, S.V. and Page, T.F., in Thin Films: Stresses and Mechanical Properties VI, edited by Gerberich, W.W., Sundgren, J-E., Gao, H., and Baker, S.P. (Mater. Res. Soc. Symp. Proc. 436, Pittsburgh, PA, 1997), p. 171.Google Scholar
18McGurk, M.R. and Page, T.F., J. Mater. Res. 14, 2283 (1999).CrossRefGoogle Scholar
19Tsui, T.Y., Oliver, W.C., and Pharr, G.M., in Thin Films: Stresses and Mechanical Properties VI, edited by Gerberich, W.W., Sundgren, J-E., Gao, H., and Baker, S.P. (Mater. Res. Soc. Symp. Proc. 436, Pittsburgh, PA, 1997), p. 207.Google Scholar
20Sneddon, I.N., Int. J. Eng. Sci. 3, 47 (1965).CrossRefGoogle Scholar
21Bolshakov, A., Oliver, W.C., and Pharr, G.M., in Thin Films: Stresses and Mechanical Properties VI, edited by Gerberich, W.W., Sundgren, J-E., Gao, H., and Baker, S.P. (Mater. Res. Soc. Symp. Proc. 436, Pittsburgh, PA, 1997), p. 141.Google Scholar
22Bolshakov, A. and Pharr, G.M., J. Mater. Res. 13, 1049 (1998).CrossRefGoogle Scholar
23Hay, J.C. and Pharr, G.M., in Fundamentals of Nanoindentation and Nanotribology, edited by Moody, N.R., Gerberich, W.W., Burnham, N., and Baker, S.P. (Mater. Res. Soc. Symp. Proc. 522, Warrendale, PA, 1998), p. 39.Google Scholar
24Hay, J.C., Bolshakov, A., and Pharr, G.M., J. Mater. Res. 14, 2296 (1999).CrossRefGoogle Scholar
25Franks, J., Enke, K., and Richardt, A., Metals and Materials 11, 695 (1990).Google Scholar
26Ham, M. and Lou, A., J.Vac. Sci. Technol. A8, 2143 (1990).CrossRefGoogle Scholar
27Raveh, A., Martinu, L., Hawthorne, H.M., and Wertheimer, M.R., Surf. Coat. Technol. 58, 45 (1993).CrossRefGoogle Scholar
28Matthews, A., Leyland, A., Holmberg, K., and Ronkainen, H., Surf. Coat. Technol. 100–101, 1 (1998).CrossRefGoogle Scholar