Microstructures of a-axis oriented YBCO films made by hybrid plasma sputtering

Published online by Cambridge University Press:  03 March 2011

W. Ito
Affiliation:
Superconductivity Research Laboratory, ISTEC, 10-13 Shinonome l chome, Koto-ku, Tokyo 135, Japan
A. Oishi
Affiliation:
Superconductivity Research Laboratory, ISTEC, 10-13 Shinonome l chome, Koto-ku, Tokyo 135, Japan
S. Mahajan
Affiliation:
Superconductivity Research Laboratory, ISTEC, 10-13 Shinonome l chome, Koto-ku, Tokyo 135, Japan
Y. Yoshida
Affiliation:
Superconductivity Research Laboratory, ISTEC, 10-13 Shinonome l chome, Koto-ku, Tokyo 135, Japan
T. Morishita
Affiliation:
Superconductivity Research Laboratory, ISTEC, 10-13 Shinonome l chome, Koto-ku, Tokyo 135, Japan
Get access

Abstract

Microstructures of a-axis oriented YBa2Cu3O7−x films made by newly developed de 100 MHz hybrid plasma sputtering were investigated using transmission electron microscopy (TEM). The films deposited on (110) NdGaO3 and (100) SrTiO3 substrates were found to grow in a perfect epitaxial fashion and with clear interface. The plan view of the TEM image showed that both films were comprised of two kinds of grains having the c axis aligning along two perpendicular directions in the plane with equal probability. The structures of the grain boundary, however, were found to be very different for the two films from the plan views. The film on NdGaO3 showed a lot of twist boundaries, while the film on SrTiO3 consisted of many symmetrical tilt boundaries and basal-plane-faced tilt boundaries. The type of grain boundary is determined by the anisotropic growth rates of the film between c direction and a-b direction.

Type
Articles
Copyright
Copyright © Materials Research Society 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1Ito, W., Oishi, A., Okayama, S., Yoshida, Y., Homma, N., and Morishita, T., Physica (Amsterdam) 204C, 295 (1993).Google Scholar
2Stoffel, N. G., Morris, P. A., Bonner, W. A., and Wilkens, B. J., Phys. Rev. B 37, 2297 (1988).Google Scholar
3Sodtke, E. and Münder, H., Appl. Phys. Lett. 60 (13), 1630 (1992).CrossRefGoogle Scholar
4Inam, A., Rogers, C. T., Remschnig, R., Farrow, L., Hart, D., Venkatesan, T., and Wilkens, B., Appl. Phys. Lett. 57 (23), 2484 (1990).Google Scholar
5Eom, C. B., Marshall, A. F., Laderman, S. S., Jacowitz, R. D., and Geralle, T. H., Science 249, 1549 (1990).CrossRefGoogle Scholar
6Basu, S. N., Carim, A. H., and Mitchell, T. E., J. Mater. Res. 6, 1823 (1991).CrossRefGoogle Scholar
7Sasaura, M., Miyazawa, S., and Mukaida, M., J. Appl. Phys. 68 (7), 3643 (1990).Google Scholar
8Scherer, T., Marienhoff, P., Herwig, R., Neuhaus, M., and Jutzi, W., Physica (Amsterdam) 197C, 79 (1992).Google Scholar
9Young, K. H. and Sun, J. Z., Appl. Phys. Lett. 59 (19), 2448 (1991).Google Scholar
10Mukaida, M. and Miyazawa, S., Jpn. J. Appl. Phys. 31 (10), 3317 (1992).CrossRefGoogle Scholar
11Marshall, A. F. and Eom, C. B., Physica (Amsterdam) 207C, 239 (1993).Google Scholar
12Iliev, M., Thomsen, C., Hadjiev, V., and Cardona, M., Phys. Rev. B 47, 1241 (1993).Google Scholar