Hostname: page-component-68c7f8b79f-kpv4p Total loading time: 0 Render date: 2025-12-17T06:47:17.541Z Has data issue: false hasContentIssue false

Simplified method for analyzing nanoindentation data and evaluating performance of nanoindentation instruments

Published online by Cambridge University Press:  31 January 2011

Takeshi Sawa
Affiliation:
Department of Mechanical Engineering, Nagaoka University of Technology, 1603–1 Kamitomioka, Nagaoka, Niigata, 940–2188 Japan
Kohichi Tanaka
Affiliation:
Department of Mechanical Engineering, Nagaoka University of Technology, 1603–1 Kamitomioka, Nagaoka, Niigata, 940–2188 Japan
Get access

Abstract

Nanoindentation is a simple and effective means for evaluating the mechanical properties of thin films. In such circumstances, nanoindentation testers have been developed and commercialized by some companies. In this study, we tested the standard four specimens using six different types of testers and established a method to evaluate the nanoindentation data. The method requires only two correction factors; one is the frame compliance, Cf, of the testers, and the other is the error of the detection of the original surface which includes both the truncation of the indenter apex and the damage of the surface caused by the preloading of the indenter. The latter correction is conducted by adding a correction length, ΔhC, to the measured penetration depth, h. It was found that the values ΔhC increase with decrease in the hardness of material and are very sensitive to the performance of the testers.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Doerner., M.F. and Nix., W.D., J. Mater. Res. 1, 601 (1986).CrossRefGoogle Scholar
2.Sneddon., I.N., Int. J. Eng. Sci. 3, 45 (1965).CrossRefGoogle Scholar
3.King., R.B., Int. J. Solids Struct. 23, 1657 (1987).CrossRefGoogle Scholar
4.Oliver., W.C. and Pharr., G.M., J. Mater. Res. 7, 1564 (1992).CrossRefGoogle Scholar
5.Woirgrad, J. and Dargenton, J-C., J. Mater. Res. 12, 2455 (1997).CrossRefGoogle Scholar
6.Murakami, Y., Tanaka, K., Itokazu, M., and Shimamoto, A., Philos. Mag. A 69, 1131 (1994).CrossRefGoogle Scholar
7.Shimamoto, A., Tanaka, K., Akiyama, Y., and Yoshizaki, H., Philos. Mag. A 74, 1097 (1996).CrossRefGoogle Scholar
8.nenpyo, Rika (Chronological Scientific Tables), 55th ed., edited by the National Astonomical Observatory of Japan (Maruzen, Tokyo, 1982).Google Scholar
9.Ashby, M.F. and Jones, D.R.H., Eng. Mater. 1 (1980).Google Scholar
10.Material Information (Corning, Corning, NY, 1999).Google Scholar
11.Simmons, G. and Wang, H., Single Crystal Elastic Constants and Calculated Aggregate Properties: A Handbook, 2nd ed. (MIT Press, Cambridge, MA, 1971).Google Scholar
12.Field., J.E., The Properties of Diamond (Academic Press, London, United Kingdom, 1979).Google Scholar
13.Shimada, M. and Ihara, I. (private communications).Google Scholar
14.Shimamoto, A. and Tanaka, K., Rev. Sci. Instrum. 68, 3494 (1997).CrossRefGoogle Scholar
15.Tanaka, K., Nishimori, K., Maeda, K., and Hotta, M., Trans. ASME, J. Tribol. 114, 274 (1992).CrossRefGoogle Scholar
16.McElhaney., K.W., Vlassak., J.J., and Nix., W.D., J. Mater. Res. 13, 1300 (1998).CrossRefGoogle Scholar
17. ISO/JIS 6507-1, Tokyo, Japan: Metallic materials-Vickers hardness test (International Organization for Standardization, 1995), Part 1.Google Scholar