Hostname: page-component-68c7f8b79f-kpv4p Total loading time: 0 Render date: 2025-12-21T23:14:36.472Z Has data issue: false hasContentIssue false

Using differential scanning calorimetry to characterize the precipitation and dissolution of V(CN) and VC particles during continuous casting and reheating process

Published online by Cambridge University Press:  26 June 2018

Mujun Long*
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Tao Liu
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Huabiao Chen*
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Dengfu Chen*
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Huamei Duan
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Helin Fan
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Kai Tan
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
Wenjie He*
Affiliation:
Laboratory of Metallurgy and Materials, College of Materials Science and Engineering, Chongqing University, Chongqing 400044, People’s Republic of China
*
a)Address all correspondence to these authors. e-mail: longmujun@cqu.edu.cn
Get access

Abstract

In this work, differential scanning calorimetry (DSC) was used to characterize and analyze the precipitation/dissolution kinetics of second phase particles during the cooling/reheating process in a vanadium microalloyed steel. The results indicated that three obvious exothermic peaks were detected on the cooling DSC curve. Furthermore, three corresponding endothermic peaks were also detected on the heating DSC curve. Combined with thermodynamic calculation and transmission electron microscopy analysis, these three exothermic peaks along cooling DSC curve were defined as the precipitation reaction of V(CN), the reaction of austenite transformation into ferrite and the precipitation reaction of VC, respectively. Meanwhile, three corresponding reverse reactions for cooling were also defined along the reheating DSC curve. The linear regression result revealed that the precipitation activation energies for V(CN) and VC were identified as 311.2 kJ/mol and 167.6 kJ/mol, respectively. The dissolution activation energies for VC and V(CN) were identified as 255.4 kJ/mol and 592.6 kJ/mol, respectively.

Information

Type
Article
Copyright
Copyright © Materials Research Society 2018 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Izotov, V.I., Komkov, N.A., and Filippov, G.A.: Morphology and crystal geometry of precipitates of a copper-containing phase and the precipitation hardening of Fe–C–Mn–Cu and Fe–C–Mn–Cu–V pearlitic steels. Phys. Met. Metallogr. 116, 37 (2015).CrossRefGoogle Scholar
Jung, J.G., Park, J.S., Kim, J., and Lee, Y.K.: Carbide precipitation kinetics in austenite of a Nb–Ti–V microalloyed steel. Mater. Sci. Eng., A 528, 5529 (2011).CrossRefGoogle Scholar
Gomez, M., Valles, P., and Medina, S.F.: Evolution of microstructure and precipitation state during thermomechanical processing of a X80 microalloyed steel. Mater. Sci. Eng., A 528, 4761 (2011).CrossRefGoogle Scholar
Ormandy, J.P., Strangwood, M., and Davis, C.L.: Effect of microalloying additions on steel plate to pipe property variations during UOE linepipe processing. Met. Sci. J. 19, 595 (2013).Google Scholar
Speer, J.G., Michael, J.R., and Hansen, S.S.: Carbonitride precipitation in niobium/vanadium microalloyed steels. Metall. Trans. A 18, 211 (1987).CrossRefGoogle Scholar
Ghosh, P., Ghosh, C., and Ray, R.K.: Thermodynamics of precipitation and textural development in batch-annealed interstitial-free high-strength steels. Acta Mater. 58, 3842 (2010).CrossRefGoogle Scholar
Shanmugam, S., Tanniru, M., Misra, R.D.K., Panda, D., and Jansto, S.: Precipitation in V bearing microalloyed steel containing low concentrations of Ti and Nb. Met. Sci. J. 21, 883 (2013).Google Scholar
Wu, H., Ju, B., Tang, D., Hu, R., Guo, A., Kang, Q., and Wang, D.: Effect of Nb addition on the microstructure and mechanical properties of an 1800 MPa ultrahigh strength steel. Mater. Sci. Eng., A 622, 61 (2015).CrossRefGoogle Scholar
Mintz, B.: Influence of nitrogen on hot ductility of steels and its relationship to problem of transverse cracking. Ironmaking Steelmaking 27, 343 (2014).CrossRefGoogle Scholar
Mejía, I., Salas-Reyes, A.E., Bedolla-Jacuinde, A., Calvo, J., and Cabrera, J.M.: Effect of Nb and Mo on the hot ductility behavior of a high-manganese austenitic Fe–21Mn–1.3Al–1.5Si–0.5C TWIP steel. Mater. Sci. Eng., A 616, 229 (2014).CrossRefGoogle Scholar
Dong, Z., Li, W., Long, M., Gui, L., Chen, D., Huang, Y., and Vitos, L.: Effect of temperature reversion on hot ductility and flow stress–strain curves of C–Mn continuously cast steels. Metall. Mater. Trans. B 46, 1 (2015).CrossRefGoogle Scholar
Mintz, B., Yue, S., and Jonas, J.J.: Hot ductility of steels and its relationship to the problem of transverse cracking during continuous casting. Metall. Rev. 36, 187 (1991).CrossRefGoogle Scholar
Cho, K.C., Dong, J.M., Yang, M.K., and Lee, J.S.: Effect of niobium and titanium addition on the hot ductility of boron containing steel. Mater. Sci. Eng., A 528, 3556 (2011).CrossRefGoogle Scholar
Salas-Reyes, A.E., Mejía, I., Bedolla-Jacuinde, A., Boulaajaj, A., Calvo, J., and Cabrera, J.M.: Hot ductility behavior of high-Mn austenitic Fe–22Mn–1.5Al–1.5Si–0.45C TWIP steels microalloyed with Ti and V. Mater. Sci. Eng., A 611, 77 (2014).CrossRefGoogle Scholar
Pierson, H.O.: Handbook of Refractory Carbides & Nitrides (Noyes Publications, Norwich, New York 1996).Google Scholar
Ma, F.J., Wen, G.H., Tang, P., Yu, X., Li, J.Y., Xu, G.D., and Mei, F.: Causes of transverse corner cracks in microalloyed steel in vertical bending continuous slab casters. Ironmak. Steelmak. 37, 73 (2010).CrossRefGoogle Scholar
Muller, C-E.: Precipitation during continuous casting (Technische Universität Berlin, Berlin, Germany 2015).Google Scholar
Yan, W., Shan, Y.Y., and Yang, K.: Effect of TiN inclusions on the impact toughness of low-carbon microalloyed steels. Metall. Mater. Trans. A 37, 2147 (2006).CrossRefGoogle Scholar
Ren, L., Zhu, J., Nan, L., and Yang, K.: Differential scanning calorimetry analysis on Cu precipitation in a high Cu austenitic stainless steel. Mater. Des. 32, 3980 (2011).CrossRefGoogle Scholar
Colombo, S., Battaini, P., and Airoldi, G.: Precipitation kinetics in Ag–7.5 wt% Cu alloy studied by isothermal DSC and electrical-resistance measurements. J. Alloys Compd. 437, 107 (2007).CrossRefGoogle Scholar
Son, S.K., Takeda, M., Mitome, M., Bando, Y., and Endo, T.: Precipitation behavior of an Al–Cu alloy during isothermal aging at low temperatures. Mater. Lett. 59, 629 (2005).CrossRefGoogle Scholar
Chang, S.H. and Wu, S.K.: Effect of cooling rate on transformation temperature measurements of Ti50Ni50 alloy by differential scanning calorimetry and dynamic mechanical analysis. Mater. Charact. 59, 987 (2008).CrossRefGoogle Scholar
Liu, M., Wu, Z., Yang, R., Wei, J., Yu, Y., Skaret, P.C., and Roven, H.J.: DSC analyses of static and dynamic precipitation of an Al–Mg–Si–Cu aluminum alloy. Prog. Nat. Sci.: Mater. Int. 25, 153 (2015).CrossRefGoogle Scholar
Falahati, A., Jun, W.U., Lang, P., Ahmadi, M.R., Povoden-Karadeniz, E., and Kozeschnik, E.: Assessment of parameters for precipitation simulation of heat treatable aluminum alloys using differential scanning calorimetry. Trans. Nonferrous Met. Soc. China 24, 2157 (2014).CrossRefGoogle Scholar
Long, M., Dong, Z., Chen, D., Zhang, X., and Zhang, L.: Influence of cooling rate on austenite transformation and contraction of continuously cast steels. Ironmak. Steelmak. 42, 282 (2015).CrossRefGoogle Scholar
Ohnaka, I.: Mathematical analysis of solute redistribution during solidification with diffusion in solid phase. Trans. Iron Steel Inst. Jpn. 26, 1045 (1986).CrossRefGoogle Scholar
Yukun, L., Guangmin, S., Zhenhua, H., and Haofei, X.: Analysis on high-temperature precipitation behavior of V–N microalloyed anti-seismic rebars. J. Cent. S. Univ. 45, 2596 (2014).Google Scholar
Primig, S. and Leitner, H.: Separation of overlapping retained austenite decomposition and cementite precipitation reactions during tempering of martensitic steel by means of thermal analysis. Thermochim. Acta 526, 111 (2011).CrossRefGoogle Scholar
Ghosh, K.S. and Gao, N.: Determination of kinetic parameters from calorimetric study of solid state reactions in 7150 Al–Zn–Mg alloy. Trans. Nonferrous Met. Soc. China 21, 1199 (2011).CrossRefGoogle Scholar
Rai, A.K., Raju, S., Jeyaganesh, B., Mohandas, E., Sudha, R., and Ganesan, V.: Effect of heating and cooling rate on the kinetics of allotropic phase changes in uranium: A differential scanning calorimetry study. J. Nucl. Mater. 383, 215 (2009).CrossRefGoogle Scholar
Málek, J.: The applicability of Johnson–Mehl–Avrami model in the thermal analysis of the crystallization kinetics of glasses. Thermochim. Acta 267, 61 (1995).CrossRefGoogle Scholar
Starink, M.J.: Analysis of aluminium based alloys by calorimetry: Quantitative analysis of reactions and reaction kinetics. ChemInform 36, 191 (2005).CrossRefGoogle Scholar
Azghandi, S.H.M., Ahmadabadi, V.G., Raoofian, I., Fazeli, F., Zare, M., Zabett, A., and Reihani, H.: Investigation on decomposition behavior of austenite under continuous cooling in vanadium microalloyed steel (30MSV6). Mater. Des. 88, 751 (2015).CrossRefGoogle Scholar
Baosheng, X., Qingwu, C., Wei, Y., Jiaming, C., and Yunfeng, Y.: Ferrite transformation kinetics of X70 pipeline steel during continuous cooling. Heat Treat. Met. 39, 83 (2014).Google Scholar
Hillert, M. and Höglund, L.: Mobility of α/γ phase interfaces in Fe alloys. Scr. Mater. 54, 1259 (2006).CrossRefGoogle Scholar
Liu, Y., Wang, D., Sommer, F., and Mittemeijer, E.J.: Isothermal austenite–ferrite transformation of Fe–0.04 at.% C alloy: Dilatometric measurement and kinetic analysis. Acta Mater. 56, 3833 (2008).CrossRefGoogle Scholar
Yong, Q.: Secondary Phases in Steels (Metallurgical Industry Press, Beijing, China, 2006).Google Scholar